DAMC, LBG, LBN, LNG Parts
























Compare DAMC, LBG, LBN, LNG
Key specifications of the parts listed on this page, taken from the manufacturer's data sheets.
| MPN | Size | Product weight | Material mounting | Corrosion resistance class CRC | Ambient temperature |
|---|---|---|---|---|---|
| LZF-63 | 63 | 14.55 oz | Galvanised steel | — | — |
| LZF-25 | 25 | 2.26 oz | Galvanised steel | — | — |
| LNZG-320 | 320 | 6810 g | Steel, Galvanised | 1 - Low corrosion stress | -20, 100 °C |
| LSNG-200 | 200 | 7368 g | Spheroidal graphite cast iron | 1 - Low corrosion stress | -40, 150 °C |
| LSNG-160 | 160 | 6001 g | Spheroidal graphite cast iron | 1 - Low corrosion stress | -40, 150 °C |
| LNZG-16 | 16 | 26 g | Wrought aluminium alloy | 2 - Moderate corrosion stress | -40, 80 °C |
| LNZG-100/125 | 100/125 | 306 g | Wrought aluminium alloy | 2 - Moderate corrosion stress | -40, 80 °C |
| LNZG-63/80 | 63/80 | 178 g | Wrought aluminium alloy | 2 - Moderate corrosion stress | -40, 80 °C |
| LBG-125-R3 | 125 | 4140 g | High-alloy stainless steel | 3 - high corrosion stress | -40, 150 °C |
| LBG-100-R3 | 100 | 1375 g | High-alloy stainless steel | 3 - high corrosion stress | -40, 150 °C |
| CRLBN-32 | 32 | 106 g | High-alloy stainless steel | 4 - Very high corrosion stress | -40, 150 °C |
| CRLNG-125 | 125 | 2539 g | Electropolished, High-alloy steel | 4 - Very high corrosion stress | -40, 80 °C |
| CRLNZG-40/50 | 40/50 | 323 g | High-alloy stainless steel | 4 - Very high corrosion stress | -40, 150 °C |
| CRLBN-20/25 | 20/25 | 82 g | High-alloy stainless steel | 4 - Very high corrosion stress | -40, 150 °C |
| CRLNG-32 | 32 | 133 g | Electropolished, High-alloy steel | 4 - Very high corrosion stress | -40, 80 °C |
| LBG-63-R3 | 63 | 580 g | High-alloy stainless steel | 3 - high corrosion stress | -40, 150 °C |
| LBG-40-R3 | 40 | 300 g | High-alloy stainless steel | 3 - high corrosion stress | -40, 150 °C |
| CRLNZG-63/80 | 63/80 | 435 g | High-alloy stainless steel | 4 - Very high corrosion stress | -40, 150 °C |
| CRLNZG-32 | 32 | 205 g | High-alloy stainless steel | 4 - Very high corrosion stress | -40, 150 °C |
| LBG-80-R3 | 80 | 1050 g | High-alloy stainless steel | 3 - high corrosion stress | -40, 150 °C |
| CRLBN-50/63 | 50/63 | 293 g | High-alloy stainless steel | 4 - Very high corrosion stress | -40, 150 °C |
| LBG-50-R3 | 50 | 540 g | High-alloy stainless steel | 3 - high corrosion stress | -40, 150 °C |
| LBG-32-R3 | 32 | 220 g | High-alloy stainless steel | 3 - high corrosion stress | -40, 150 °C |
| CRLBN-40 | 40 | 185 g | High-alloy stainless steel | 4 - Very high corrosion stress | -40, 150 °C |